Strength Behavior of Veneered Zirconia after Different Surface Treatments
Keywords:
flexural strength; all-ceramics; Y-TZP; delamination
Abstract
Abstract not found
Downloads
- Article PDF
- TEI XML Kaleidoscope (download in zip)* (Beta by AI)
- Lens* NISO JATS XML (Beta by AI)
- HTML Kaleidoscope* (Beta by AI)
- DBK XML Kaleidoscope (download in zip)* (Beta by AI)
- LaTeX pdf Kaleidoscope* (Beta by AI)
- EPUB Kaleidoscope* (Beta by AI)
- MD Kaleidoscope* (Beta by AI)
- FO Kaleidoscope* (Beta by AI)
- BIB Kaleidoscope* (Beta by AI)
- LaTeX Kaleidoscope* (Beta by AI)
How to Cite
References
Moustafa Aboushelib, Hang Wang (2013) Influence of crystal structure on debonding failure of zirconia veneered restorations. 29(7), e97-e102.
Jin-Young Song, Sang-Won Park, Kwangmin Lee, Kwi-Dug Yun, Hyun-Pil Lim (2013) Fracture strength and microstructure of Y-TZP zirconia after different surface treatments. 110(4), 274-280.
H Sato, K Yamada, G Pezzotti, G Pezzotti, M Nawa, S Ban (2008) Mechanical properties of dental zirconia ceramics changed with sandblasting and heat treatment. 27, 408-414.
Y Zhang, J Kim (2009) Graded structures for damage resistant and aesthetic all-ceramic restorations. 25, 781-790.
Hideo Toraya, Masahiro Yoshimura, Shigeyuki Somiya (1984) Calibration Curve for Quantitative Analysis of the Monoclinic-Tetragonal ZrO2System by X-Ray Diffraction. 67(6), C-119-C-121.
T Kosmac, R Wagner, N Claussen (1981) X-ray determination of transformation depths in ceramics containing tetragonal ZrO 2. 64, 72-C73.
(2011) Effect of Surface Treatment Condition on Bond Strength between CAD/CAM Zirconia and Veneering Ceramics.
Published
2016-12-15
Issue
Section
License
Copyright (c) 2016 Authors and Global Journals Private Limited

This work is licensed under a Creative Commons Attribution 4.0 International License.